[TheForge] Re: TheForge digest, Vol 1 #597 - 14 msgs
Sudden Service #5
[email protected]
Tue Sep 10 23:19:01 2002
Thanks Dan, but yours isn't what we are using at the event. Flaxy is coming
up to teach us about Medieval Period iron making & we are building a clay
Scandinavian Shaft furnace type of bloomery, very low tech & no metal on
the outside. When I have some time I would love to discuss yields & such,
but I am looking for some photos to show the Fire Chief tomorrow. The
photos that were shown had on the Forge had Flaxy in them (I would get some
from her but she doesn't check her email very often).
Pax,
Olaf
----- Original Message -----
> From: "Dan Scheid" <[email protected]>
> To: <[email protected]>
> Subject: Re: [TheForge] Bloomery Photos?!
> Date: Tue, 10 Sep 2002 14:42:01 -0700
> Reply-To: [email protected]
>
> you can check out mine
> Dan Scheid
> Flying horse forge
> http://home.earthlink.net/~chevalvolant/flyinghorseforge.html
> > Hej!
> > Early August or late September someone posted on the Forge some
photos
> > of a Bloomery in use. When I tried to get access to it after Pennsic I
was
> > told it was "private". I need to show some photos to the Fire Chief to
get
> > his approval (he didn't seem to think there was a problem, but the site
is
> > just wanting to be careful & he is wanting to be through). Could some
one
> > email some photos-all mine are taken in the dark & don't give a real
ideal
> > of the size.
> > Pax,
> > Olaf