Morning Bob:

This is Ron's web site, you'll find out more than enough to build and tune
burners and links to guys selling supplies, parts and complete burners under
the Forge and Foundry link. The Jet ejectors are being called: Mongo, Side
Arm and I think T-Rex. Ralph Sproul also has pics of his Jet ejector burners
posted though the pics are really of the forge, I think they give a decent
look at the burners as well.

Remember, the easy way to tell the difference is the air intakes are at 90*
to the bore and gas jet.