hit with a grinder the best rod for the job would be 7018, 7018 don't like rust.
[email protected] wrote:Can someone recommend a good stick to use for welding rusting metal. The 1/2
wall 6" by 6" steel tube for the upright of the power hammer I am going to
build has been sitting outside for a few months and now it is rusted all over.
I am going to fill the in inside with concrete to add stability but the outside
has to have the hammer support welded to it. Clean it? Polish it? weld right
through the rust? suggestions?
Dan
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: [email protected]
password: anvil
___________
---------------------------------
Do you Yahoo!?
Y! Web Hosting - Let the expert host your web site
--- StripMime Report -- processed MIME parts ---
multipart/alternative
text/plain (text body -- kept)
text/html
The reason this message is shown is because the post was in HTML
or had an attachment. Attachments are not allowed.
Please post in Plain-Text only.---