[TheForge] hardie hole tools and swages
Justin Fisher
[email protected]
Sat Oct 19 18:25:01 2002
How did you make the cone? That sounds like a difficult project (I'm
trying to visualize how you'd use the 50# LG)
Justin
Northborough, MA
At 02:58 PM 10/19/2002 -0500, you wrote:
> The 3 I use most often are a cut off (by far the most used), a bending
>fork, and a small 2" diameter by 7" high cone. All fit in the hardy hole.
>I made them with hammer and anvil (sometimes the 50lb. Little Giant) out of
>old big truck axels (probably 4140). The bending fork and cone are not heat
>treated, just forged and used. The cut off is heat treated with water even
>though oil is suggested for hardening. There are a hundred ideas for bottom
>tools for the hardy hole (many which are quite useful depending on the
>project) shown in Otto Schmirler's book Werk und Werkzeug des Kunstschmieds
>ISBN # 3 8030 5040 5.
>
>Dick
>Grand Island, NE