I use misc. cut off scraps for media. It takes under an hour to get stuff
clean.

Bob Ehrenberger
Shelbyville, Mo

From: "Shannell Sugrue" <[email protected]>
To: <[email protected]>
Date: Wed, 16 Oct 2002 23:23:31 +0930
Subject: [TheForge] Tumbler media
Reply-To: [email protected]

I bought some commercial ceramic tumbler media for my newly built tumbler, I
love the texture and colour it leaves on parts BTW. Question for anyone, is
how long they usually tumble thier parts for? I thought the process was
quicker, took over 3 hours for some small lightly scaled candleholders and
some leaves to get to the point I was happy with them. The media Im using
has a triangular cross section and the are rectangular along the side, they
seem to slide over the parts more than collide, Im thinking of trying some
pyramid shaped ceramic media, I think they would be more aggresive.