lava rock is pretty aggressive :)    Did you put tumbler bars inside  the shell?
 Shannell Sugrue <[email protected]> wrote:I bought some commercial ceramic tumbler media for my newly built tumbler, I
love the texture and colour it leaves on parts BTW. Question for anyone, is
how long they usually tumble thier parts for? I thought the process was
quicker, took over 3 hours for some small lightly scaled candleholders and
some leaves to get to the point I was happy with them. The media Im using
has a triangular cross section and the are rectangular along the side, they
seem to slide over the parts more than collide, Im thinking of trying some
pyramid shaped ceramic media, I think they would be more aggresive.

_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: [email protected]
password: anvil
___________




---------------------------------
Do you Yahoo!?
Faith Hill - Exclusive Performances, Videos, & more
faith.yahoo.com

--- StripMime Report -- processed MIME parts ---
multipart/alternative
  text/plain (text body -- kept)
  text/html
The reason this message is shown is because the post was in HTML
or had an attachment. Attachments are not allowed.
Please post in Plain-Text only.---