I am in the process of designing a trellis in a art deco style .In order to
cut down on weight I am thinking of using aluminum any tips on forging
aluminum? I am thinking of just light surface treatment basically .
I've never really hammered allum. heat or no heat? if I use brass or bronze
as an accent is there a reaction between the metals I should be aware of?
thanks.
.
----- Original Message -----
From: Howell Steve <[email protected]>
To: <[email protected]>
Sent: Monday, October 07, 2002 10:34 AM
Subject: RE: [TheForge] spoon swages
> Robert polling in ohio : 614-653-9199
> Or his neighbor Norman wendell 614-654-2040
>
> Been a while since I called them and the area code might've changed. I'm
thrilled with their little swages and would like to try some of their drifts
as well.
>
> Good luck,
> Steve
>
> -----Original Message-----
> From: [email protected] [mailto:[email protected]]
> Sent: Monday, October 07, 2002 9:38 AM
> To: [email protected]
> Subject: [TheForge] spoon swages
>
>
> i'm looking for some spoon swages. seems like a while back some were
mentioned. anybody know?
>
> thanks
>
> bob schade
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed.
> Please post in Plain-Text only.---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>