For the stuff I do I found that the Harbor Frieght bender was worth the cost
and I also got the setup for doing scroll work. They also have a jig for
doing twisting but I did not get that piece yet. I nice thing about it is I
have it mounted to a 3' dia piece from a cable spool. It has all of the basic
tools and if a person needed special dies they could get them froom
hossfield. It is the same as the number one. Mine came through the mail
system and now we have a Harbor Freight in Phoenix. Good place to get cheap
tools that can last for awhile. My bender is over 7 years old and sits
outside all the time. Keep dies in storage until I need them.
They also have a bench top one too.
Later Ike
Pan's Forge