> On my regular Kinyon style air hammer I had brass for the guides as is called
> for in the plans but have since switched over to the UHMW platic and believe
> it is a much better hammer now.It is faster and I do not have to oil the
> guides like I did when I had brass and the temp (I live where it gets cold)
> does not seem to effect it at all.
>
> Bob
> HotAnvil Forge
> http://members.tripod.com/hotanvil_forge
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed.
> Please post in Plain-Text only.---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>