[TheForge] Re:Hand Hacksaw blades

Fiorini & Skiles [email protected]
Sun Nov 24 08:02:00 2002


The Lenox blade is great.  I have used it for more than ten years now and
would never consider going back to another brand.  I have two hacksaws in
the shop.  One for cold work and one for hot work.   Both have Lenox blades.
Bill
----- Original Message -----
From: "Adam Whiteson" <[email protected]>
To: <[email protected]>
Sent: Saturday, November 23, 2002 7:51 PM
Subject: Re: [TheForge] Re:Hand Hacksaw blades


> I looked at some lennox blades in my local electrical supply store but
they
> only had wavy teeth patterns.   I much prefer a straight row of teeth with
> set.  Comes from my years as a  woodworker I guess.
>
> Adam
>
> At 07:54 AM 11/23/2002 -0800, you wrote:
> >Well, I finally found some Lenox blades! They are so
> >much better than Home Depot's best that I use my hand
> >hack saw where I would get out my side
> >grinabrasionaion blades before. A real time saver.
> >Thanks for the advice.
> >Lynn
> >
> >--- Stephen McGehee <[email protected]> wrote:
> > > Call your local electrical wholesale house and ask
> > > if they stock Lenox white blades.  I have used these
> > > in 24 and 32 tooth sizes for 20+ years.  Don't waste
> > > your time with Klein blades though.
> > > Stephen
> >
> >
> >__________________________________________________
> >Do you Yahoo!?
> >Yahoo! Mail Plus � Powerful. Affordable. Sign up now.
> >http://mailplus.yahoo.com
> >_______________________________________________
> >http://mailman.qth.net/mailman/listinfo/theforge
> >theforge mail list group photo site is
> >http://www.photoaccess.com
> >Login:  [email protected]
> >password:  anvil
> >___________
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>