Well, I finally found some Lenox blades! They are so
much better than Home Depot's best that I use my hand
hack saw where I would get out my side
grinabrasionaion blades before. A real time saver.
Thanks for the advice.
Lynn

--- Stephen McGehee <[email protected]> wrote:
> Call your local electrical wholesale house and ask
> if they stock Lenox white blades.  I have used these
> in 24 and 32 tooth sizes for 20+ years.  Don't waste
> your time with Klein blades though.
> Stephen