[TheForge] Jewelry Finishes

Terry L. Ridder [email protected]
Mon Nov 18 20:28:04 2002


hello;

john & bruce, would putting the piece in ash or vermiculite
slow the cooling process enough to allow it is cool slow enough
to avoid shattering?

On Mon, 18 Nov 2002, John Chobrda wrote:

john> 
john> Bruce, I tried putting glass on a forged piece a while back.
john> It looked great until it started to cool. Glass splinters
john> flying about the shop. If you had an annealing oven,
john> and could bring the piece down slowly it might work.
john> 
john> John C.
john> 

-- 
Terry L. Ridder ><>