[TheForge] Brazing vs welding

Larry and Pat Brown [email protected]
Fri Nov 15 22:02:00 2002


Any kind of flux used?
L Brown

At 09:40 AM 11/15/2002 -0700, you wrote:
>Its higher tech, higher bucks, but I use silicon bronze brazing rod all the
>time with the tig welder. It works great for brazing dissimilar metals
>together, and puts much less heat into something because of how controllable
>the tig torch is. I often use it to braze thin wall tubing, as there is much
>less distortion when you dont have to actually melt the parent metal. Tig
>brazing also really works great in those razor blade to propeller shaft type
>situations- I used to do a production candlestick where we brazed on 24 ga
>stamped steel leaves to 3/8" round, and any other technique would have
>reduced the stampings to a puddle.
>Ries Niemi
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  [email protected]
>password:  anvil
>___________