How about a demonstration of how heat affects metals, anneal something, quench and harden something, forge weld something.
Ray
Cincinnati
>
> From: "Kelloughs" <[email protected]>
> Date: 2002/11/05 Tue PM 04:41:57 EST
> To: <[email protected]>
> Subject: [TheForge] Science fair project
>
> My 10 year old son is going to do a science fair project soon. He frequently helps me at the forge and also likes to do his own little jobs. I thought that it would be a good idea to do his project on blacksmithing as no one at his school has done a project on this subject in recent past (that we know about).
> My question would be: does any one know of a good project for him, or any recourses we could use? Please keep in mind that he is ten years old, and I want him to pretty much do the job him self with only my supervision.
> Thanks in advance
> John Kellough
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed.
> Please post in Plain-Text only.---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>