Philip, Rob, et al

Sure Philip wait til after I do a test piece to tell me I was overdoing 
it .  

Well I didn't get any pictures posted, but I did get the four fame 
pieces done yesterday.  I have a new appreciation for angle iron!

Today I completed the top plate and 2 and 1/2 of the  chains.  

Looks like I'll make the Tuesday drop off to Roger.  Rob, what's the 
best place/way for Roger to get it to you  once he arrives?

I'll try to post some pictures tomorrow

Bill

Philippa Alderton wrote:

>----- Original Message ----- 
>From: "April & Bill Clemens" <[email protected]>
>To: <[email protected]>
>Sent: Tuesday, May 28, 2002 10:13 PM
>Subject: Re: [TheForge] Mastermyr - Fire Grid
>
>
>>Got the Pure Iron and did a sample corner piece.  Decided to make the 
>>hook only from the end support angle and not from the end and side. 
>>
>
>Kinda thought that might be a bit much...
>
>> Stared at the drawings and picture for a while and decided that that is 
>>most likely the way the original was.  Would love to see the original 
>>sometime.  Should have the main angle frame together sometime tomorrow. 
>> Will try to get a picture posted tomorrow on my progress..
>>
>
>I'll be waiting to see them ;-)
>
>Phlip 
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  [email protected]
>password:  anvil
>___________
>
>
>
>