[TheForge] Mastermyr - Fire Grid

April & Bill Clemens [email protected]
Mon May 27 19:24:00 2002


Rob,
I'm off to meet Roger in Harrisburg, Pa to pick up the Pure Iron Stock I 
need for the fire grid.  Will keep you posted on my daily progress. 
 Plan is to meet Roger again on morning of 4 June in Harrisburg with the 
completed piece.  Should I mark it or are all the items being 
touchmarked  theforge?

Bill

Rob Fertner wrote:

>Bless you. Pure iron is just fine.
>Thanks,
>Rob
>----- Original Message -----
>From: "April & Bill Clemens" <[email protected]>
>To: <[email protected]>
>Sent: Monday, May 27, 2002 9:14 AM
>Subject: Re: [TheForge] Mastermyr - Fire Grid
>
>
>>Rob, et al,
>>
>>After some thought and a phone call to the BGCM vice President, Roger
>>Duncan, who has a cache of pure iron; I've decided to make the fire grid
>>out of pure iron.  Just not enough time to first hammer out the needed
>>wrought iron stock and then overcome the other challenges in making the
>>fire grid.  Planning to meet Roger this evening to get the pure iron
>>after our town's Memorial Day Parade and family picnic.  The added bonus
>>is that Roger's driving out to the conference on Tuesday 4 Jun and has
>>agreed to bring the completed Fire Grid.  Will keep you posted on my
>>progress. Have a good and safe Memorial Day!
>>
>>Bill
>>
>>Rob Fertner wrote:
>>
>>>Bill,
>>>Sorry for the delayed reply, I was out of town this weekend.
>>>The absolute last minute get it to me down to the wire date
>>>would be Monday June 3rd. The 1st and 2nd I was planning to pack up
>>>everything
>>>so it was ready to go.
>>>If you can get it done, God bless you.
>>>Rob
>>>----- Original Message -----
>>>From: "April & Bill Clemens" <[email protected]>
>>>To: <[email protected]>
>>>Sent: Sunday, May 26, 2002 9:42 PM
>>>Subject: Re: [TheForge] Mastermyr - Fire Grid
>>>
>>>
>>>>Well, the best laid plans .... My daughter came to visit with my
>>>>grandson, so I didn't do as much work today as I planned.
>>>>
>>>>I did find time to make a test angle and corner hook.  Looks like it
>>>>will work fine.   Biggest problem is not having any wrought iron stock
>>>>anywhere near the dimensions I need. Because of that, the hardest part
>>>>will be hammering out the four 2" x 3/16" x 24" pieces I need for the
>>>>outside frame. Will get back to work on it on Tuesday and see how it
>>>>
>goes.
>
>>>>Haven't  heard from Rob on his drop dead date, but the email from  Jim
>>>>Sorber gave me an idea.  Is anyone from eastern PA, New Jersey, etc
>>>>that's going to the conference planning to travel through PA on
>>>>Interstate 80 on there way there?  I only live about a mile off I 80 in
>>>>central PA( Route 15 - Susquehanna River).  If anyone's going that way
>>>>and is willing to pick up the Fire Grid it might give me the time I need
>>>>to finish it.
>>>>
>>>>Bill
>>>>
>>>>April & Bill Clemens wrote:
>>>>
>>>>>Rob, Ralph,  Mike,  Phlip, and anyone else with suggestions,
>>>>>
>>>>>I've posted a picture in the "anything else" folder on Photo Access.
>>>>>It's a sketch on my idea of the corner hook detail for the Fire Grid.
>>>>>Each corner  angle would lap and be riveted.  The vertical portion of
>>>>>each angle would be drawn out and form the hook(actually two hooks
>>>>>side by side)  Best  I could determine from the sketches and photo I
>>>>>saw. Does this look right to you?
>>>>>
>>>>>For the chain links between the grid and the top plate.  Some appear
>>>>>to be hooks others welded eyes.  Should there be a mix or do you think
>>>>>they were all welded eyes originally?  Also lengths of individual
>>>>>links appear random.  Your thoughts?
>>>>>
>>>>>Rob, I plan to work on this tomorrow and will let you know by days end
>>>>>if  I think there's a chance I can complete it in time to ship to you.
>>>>>What's your absolute drop dead date to receive it?   I think I have
>>>>>enough wrought iron to make it but might have to use some pure iron.
>>>>>If I complete it should I mark it in any way or did you come up with a
>>>>>theforge mastermyr touch mark to mark all the pieces?
>>>>>
>>>>>Bill Clemens
>>>>>Hound and Hare Forge
>>>>>
>>>>>
>>>>>
>>>>>
>>>>>
>>>>>Ralph wrote:
>>>>>
>>>>>>I hope this helps.
>>>>>>
>>>>>>Frame about 50 X 50 cm: strip width 0.45 cm, thickness 0.25 cm; grid
>>>>>>rods 49.0 X 1.2 X 0.3-0.5 cm.
>>>>>>Chain links about 0.6-0.7 cm, total length of each chain about 42 cm.
>>>>>>
>
>>>>>>Swivel: four-armed plate
>>>>>>about 16 X 9 cm, thickness 0.3 cm; hook 10.3 X 1.5 X 0.7 cm; the open
>>>>>>part of the hook maximum
>>>>>>width 1.5 cm.
>>>>>>
>>>>>>Ralph
>>>>>>
>>>>>>I do not have a drop dead date. <smile> Tho Rob Fertner does. He is
>>>>>>the collection point for all the stuff as he will carry it to
>>>>>>LaCrosse. Unless you are going as well then you can give it to him
>>>>>>then. But Rob is wanting to have it first part of June.
>>>>>>
>>>>>>Ralph
>>>>>>
>>>>>>
>>>>>>
>>>>>>
>>>>>>"Good is the enemy of Excellent. Talent is not necessary for
>>>>>>
>>>Excellence.
>>>
>>>>>>Persistence is necessary for Excellence. And Persistence is a
>>>>>>
>>>Decision."
>>>
>>>>>>--- StripMime Report -- processed MIME parts ---
>>>>>>multipart/mixed
>>>>>>text/plain (text body -- kept)
>>>>>>image/jpeg
>>>>>>The reason this message is shown is because the post was in HTML
>>>>>>or had an attachment. Attachments are not allowed.
>>>>>>Please post in Plain-Text only.---
>>>>>>_______________________________________________
>>>>>>http://mailman.qth.net/mailman/listinfo/theforge
>>>>>>theforge mail list group photo site is
>>>>>>http://www.photoaccess.com
>>>>>>Login:  [email protected]
>>>>>>password:  anvil
>>>>>>___________
>>>>>>
>>>>>>
>>>>>>
>>>>>>
>>>>>_______________________________________________
>>>>>http://mailman.qth.net/mailman/listinfo/theforge
>>>>>theforge mail list group photo site is
>>>>>http://www.photoaccess.com
>>>>>Login:  [email protected]
>>>>>password:  anvil
>>>>>___________
>>>>>
>>>>>
>>>>>
>>>>>
>>>>_______________________________________________
>>>>http://mailman.qth.net/mailman/listinfo/theforge
>>>>theforge mail list group photo site is
>>>>http://www.photoaccess.com
>>>>Login:  [email protected]
>>>>password:  anvil
>>>>___________
>>>>
>>>>
>>>>
>>>
>>>_______________________________________________
>>>http://mailman.qth.net/mailman/listinfo/theforge
>>>theforge mail list group photo site is
>>>http://www.photoaccess.com
>>>Login:  [email protected]
>>>password:  anvil
>>>___________
>>>
>>>
>>>
>>>
>>
>>_______________________________________________
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login:  [email protected]
>>password:  anvil
>>___________
>>
>>
>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  [email protected]
>password:  anvil
>___________
>
>
>
>