[TheForge] Mastermyr - Fire Grid
Rob Fertner
[email protected]
Sun May 26 23:07:00 2002
Bill,
Sorry for the delayed reply, I was out of town this weekend.
The absolute last minute get it to me down to the wire date
would be Monday June 3rd. The 1st and 2nd I was planning to pack up
everything
so it was ready to go.
If you can get it done, God bless you.
Rob
----- Original Message -----
From: "April & Bill Clemens" <[email protected]>
To: <[email protected]>
Sent: Sunday, May 26, 2002 9:42 PM
Subject: Re: [TheForge] Mastermyr - Fire Grid
> Well, the best laid plans .... My daughter came to visit with my
> grandson, so I didn't do as much work today as I planned.
>
> I did find time to make a test angle and corner hook. Looks like it
> will work fine. Biggest problem is not having any wrought iron stock
> anywhere near the dimensions I need. Because of that, the hardest part
> will be hammering out the four 2" x 3/16" x 24" pieces I need for the
> outside frame. Will get back to work on it on Tuesday and see how it goes.
>
> Haven't heard from Rob on his drop dead date, but the email from Jim
> Sorber gave me an idea. Is anyone from eastern PA, New Jersey, etc
> that's going to the conference planning to travel through PA on
> Interstate 80 on there way there? I only live about a mile off I 80 in
> central PA( Route 15 - Susquehanna River). If anyone's going that way
> and is willing to pick up the Fire Grid it might give me the time I need
> to finish it.
>
> Bill
>
> April & Bill Clemens wrote:
>
> > Rob, Ralph, Mike, Phlip, and anyone else with suggestions,
> >
> > I've posted a picture in the "anything else" folder on Photo Access.
> > It's a sketch on my idea of the corner hook detail for the Fire Grid.
> > Each corner angle would lap and be riveted. The vertical portion of
> > each angle would be drawn out and form the hook(actually two hooks
> > side by side) Best I could determine from the sketches and photo I
> > saw. Does this look right to you?
> >
> > For the chain links between the grid and the top plate. Some appear
> > to be hooks others welded eyes. Should there be a mix or do you think
> > they were all welded eyes originally? Also lengths of individual
> > links appear random. Your thoughts?
> >
> > Rob, I plan to work on this tomorrow and will let you know by days end
> > if I think there's a chance I can complete it in time to ship to you.
> > What's your absolute drop dead date to receive it? I think I have
> > enough wrought iron to make it but might have to use some pure iron.
> > If I complete it should I mark it in any way or did you come up with a
> > theforge mastermyr touch mark to mark all the pieces?
> >
> > Bill Clemens
> > Hound and Hare Forge
> >
> >
> >
> >
> >
> > Ralph wrote:
> >
> >> I hope this helps.
> >>
> >> Frame about 50 X 50 cm: strip width 0.45 cm, thickness 0.25 cm; grid
> >> rods 49.0 X 1.2 X 0.3-0.5 cm.
> >> Chain links about 0.6-0.7 cm, total length of each chain about 42 cm.
> >> Swivel: four-armed plate
> >> about 16 X 9 cm, thickness 0.3 cm; hook 10.3 X 1.5 X 0.7 cm; the open
> >> part of the hook maximum
> >> width 1.5 cm.
> >>
> >> Ralph
> >>
> >> I do not have a drop dead date. <smile> Tho Rob Fertner does. He is
> >> the collection point for all the stuff as he will carry it to
> >> LaCrosse. Unless you are going as well then you can give it to him
> >> then. But Rob is wanting to have it first part of June.
> >>
> >> Ralph
> >>
> >>
> >>
> >>
> >> "Good is the enemy of Excellent. Talent is not necessary for
Excellence.
> >> Persistence is necessary for Excellence. And Persistence is a
Decision."
> >>
> >>
> >> --- StripMime Report -- processed MIME parts ---
> >> multipart/mixed
> >> text/plain (text body -- kept)
> >> image/jpeg
> >> The reason this message is shown is because the post was in HTML
> >> or had an attachment. Attachments are not allowed.
> >> Please post in Plain-Text only.---
> >> _______________________________________________
> >> http://mailman.qth.net/mailman/listinfo/theforge
> >> theforge mail list group photo site is
> >> http://www.photoaccess.com
> >> Login: [email protected]
> >> password: anvil
> >> ___________
> >>
> >>
> >>
> >>
> >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
> >
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>