Sat May 25 10:33:00 2002
>
>Does anyone know how the corners were put together?
No I do not. But I was planing on small rivets.
>Am I remembering correctly that the "wire running around the frame was
>intended as a later reinforcement?
Yes the wire was added by the museum to keep it all together and in proper
orientation.
>Since I don't have the book, can anyone tell me where the artifact is now?
I believe it is in a museum in Sweden....
>Phlip I figure if I know where it is, I might be able to ask the curator a
>few questions....
>
>
>-