> GHS wrote:
> >
> > an any one direct me to a picture or
> > sketch of the fire grid? The site that I
> > have bookmarked has a broken link to
> > that item.
> >
> > Mike Graf
>
> Mike,
> I will email you later today with what info I have on the grid. I used
> to have the book, but some how I have misplaced it.
> If you can do teh grid that would be way cool, and highly appreciated by
> me.
>
> basic grid is 50 cm square with 9 bars across and one center bar cross
> wise from the 9. Has what looks to be like a survey style link from each
> corner connected to a cross piece with a loop thru the center. The outer
> edge of the grid looks like angle iron. That is the hardest part to do,
> in my opinion.
> A scaned pic and detailed words will be in my later email.
>
> Ralph