What type of axe? Why not fold and forge weld for the axe? Only the
edge would have to be high carbon then as well.
John
Lynn Emrich wrote:
> Hope for a little advice from you guys (male and
> female) for a little problem with smiting.
>
> I've been pounding out knives and the occasional sword
> for a couple of years but I thought I'd try my hand
> with an axe. I used a leaf spring, 1/2" X 3" and tried
> to upset for a handle. What I got was either cold
> shuts or when I pounded out during the process of
> trying to upset, it got too long and not enough thick
> enough for a handle.
>
> All this was done by hand, so you know I have a sore
> arm. Couldn't pick up the 6# hammer at the end and
> tried to use the 4#. I'll try again tomorrow.
>
> Thanks, Lynn
>
> __________________________________________________
> Do You Yahoo!?
> LAUNCH - Your Yahoo! Music Experience
> http://launch.yahoo.com
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________