i was thinking of welding a hard face directly on the A36. not welding a plate on. i figured if they can weld a hard face on rock crushers that it would work okay for dies used on hot metal.
i may just try the A36 as is or superquenched as dan mentioned.
thanks.
bob
______
>Yeah it would work if you have to, but its better to use a solid die if you
>ask me, i find gaps between dies and the anvil mean less of a transfer of
>impact is possible. Why not just use A36 for the dies, I have several mild
>steel dies and they work fine, some are super quenched some arent, some are
>used quite a bit. Why not use flat dies with a saddle setup so you can use
>the harder metal dies when you want them and you can change them around.
>
>----- Original Message -----
>From: <[email protected]>
>To: <[email protected]>
>Sent: Thursday, May 02, 2002 9:45 PM
>Subject: [TheForge] hard faced dies
>
>
>>
>> would it work to weld a hard face on A36 to make air hammer dies? if so
>any rod recommendations. if not why?
>>
>> thanks.
>>
>> bob
>>
>>
>> _______________________________________________
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: [email protected]
>> password: anvil
>> ___________
>>
>>
>>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________