[TheForge] copper arch
Ralph Sproul
[email protected]
Wed May 1 21:43:00 2002
I'll probably start with the muriatic and phosphoric to see how fast
they work. I have some test pieces as the aftermath is sometimes not
wonderful with acids.
From there I'd probably go the flour, vinegar, and salt for a mild
abrasion and maybe use them with the Brillo pads. The paste might be nice
as some of the copper cleaners were pretty neat pastes, but you didn't get
much mileage out of a $4 bottle.
Ralph
----- Original Message -----
From: "April & Bill Clemens" <[email protected]>
To: <[email protected]>
Sent: Wednesday, May 01, 2002 9:28 PM
Subject: Re: [TheForge] copper arch
> I'll wait for your results report. Which of the 9 are you trying?
>
> Bill Clemens
>
> Ralph Sproul wrote:
>
> > Thanks for all the suggestions on how to clean up the copper.
I've
> >picked up some of the items to try out tommorrow.
Interesting........nine
> >different suggestions.
> >
> > Muriatic acid (with no steel contact previously)
> > Lemons with salt
> > Brillo pads
> > Ketchup
> > Soy Sauce
> > Salt & Vinegar
> > Vinegar/Salt/Wheat Flour
> > Sodium Bisulfate
> > Phosphoric Acid
> >
> > Just for those of you that want to print a list to try yourself
> >sometime.
> >
> >Ralph
> >
> >_______________________________________________
> >http://mailman.qth.net/mailman/listinfo/theforge
> >theforge mail list group photo site is
> >http://www.photoaccess.com
> >Login: [email protected]
> >password: anvil
> >___________
> >
> >
> >
> >
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>