[TheForge] copper arch
Ralph Sproul
[email protected]
Wed May 1 21:36:01 2002
Yeah, when I looked at the recipe, I had to go buy the lemons, soy
sauce, ketchup and wheat flour, the rest of the stuff I had on hand. :-)
Ralph
----- Original Message -----
From: "Philippa Alderton" <[email protected]>
To: <[email protected]>
Sent: Wednesday, May 01, 2002 9:07 PM
Subject: Re: [TheForge] copper arch
> Jeeze- while you're at it, fry up some burgers, and lets have a cook-out!
> Half that stuff would go well with a goos meal- a copper cleaning party
!!!
>
> Phlip
>
> ----- Original Message -----
> From: "Ralph Sproul" <[email protected]>
> To: <[email protected]>
> Sent: Wednesday, May 01, 2002 8:59 PM
> Subject: [TheForge] copper arch
>
>
> > Thanks for all the suggestions on how to clean up the copper.
> I've
> > picked up some of the items to try out tommorrow.
Interesting........nine
> > different suggestions.
> >
> > Muriatic acid (with no steel contact previously)
> > Lemons with salt
> > Brillo pads
> > Ketchup
> > Soy Sauce
> > Salt & Vinegar
> > Vinegar/Salt/Wheat Flour
> > Sodium Bisulfate
> > Phosphoric Acid
> >
> > Just for those of you that want to print a list to try yourself
> > sometime.
> >
> > Ralph
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>