[TheForge] propane forge

Roy Wilson [email protected]
Sun Mar 31 14:32:01 2002


On Sun, 31 Mar 2002 14:12:21 -0500, [email protected] wrote:

>Although I'm no pro, I beg to differ with Roy, two of the most efficient forges I've seen are the Swan Mini Mother and the Sandia neither one of them have a swirling flame. When I say efficient you must take that with a grain of salt, I have not seen the lab test results.

  I was talking gas consumption for equivalent heat over equivalent
times.



Roy Wilson
General Operations Director
Zanzibar Internet Land Line Administrator

<[email protected]>