[TheForge] Finishing Pure Iron
Dave Brown
[email protected]
Sat Mar 30 09:03:00 2002
At 07:54 03/30/02 -0600, you wrote:
>>Is there any difference between the finihsing that is
>>required for pure iron and for mild steel. Does it
>>oxide differently? Do the oil and wax finishes still
>>work?Does it last any longer in the weather?
>
>Frederick,
I forgot to complete this thought:
>Combining these two thought: If low carbon content results in low
>oxidation rates, and old finishing oils/waxes will adhere as well, then
>the final result sounds better than what you'd get using mild steel.
With low corrosion properties, if the piece does start to rust under the
finish, I don't think you'll get the same level of 'creeping rust' under
the finish that you get with mild steel.
>Make sense? Does to me, but I could be misremembering or way out on a
>limb with my logic.
>
>Dave Brown