[TheForge] 4140 vs 4340

Dave Brown [email protected]
Wed Mar 27 21:21:00 2002


At 20:47 03/27/02 -0500, you wrote:

>How hot would you temper those dies Grant?  You mentioned "the book " what 
>book
>would you recommend for heat treating information?
>
>John Newman

John,

I know I'm not Grant and your question was directed to him.  But ... you 
can get the basic heat treating information from the Principal Metals site:

http://www.principalmetals.com/properties/result.asp?Family=Alloy+Steels&MetalName=4340

The Principal Metals site (http://www.principalmetals.com/) has a lot of 
good basic information about various alloys of steel and other metals.

It's worth bookmarking in your browser.

Dave