For mechanical cleaning I use a cup brush on the angle grinder. If you have a self cleaning oven you can put it inside and run through a clean cycle it comes out very clean, everything gets burned off. I guess you could heat it on the forge until it glows and get the same result. Once clean season well with vegetable oil. Bob Ehrenberger Shelbyville, Mo