On Wed, 27 Mar 2002 06:13:45 -0600, Dave Brown wrote:

>>ok I remember a post of gluing two pieces together to hold them  so you
>>could weld them  anyone remember this ? if so what glue?
>>Dan Scheid
>>Flying horse forge
>
>Dan - If I remember correctly it was just krazy glue or other super glue 
>type of stuff.  This is NOT for forge welding but I think I remember 
>someone said that it would hold for tacking something together for arc 
>welding then will burn out in the forge if you plan on finishing the 
>welding in the forge.  Not too sure about this last part - memory failing ....

	Memory worked fine on that one.  Krazy glue for very smooth
surfaces, the arc or flame will burn it out just fine.  JB Weld or
other putty epoxies for tacking parts together that have rough
surfaces.  Got to keep it out of the way of the arc, or it'll mess
up your weld line.

	But much handier than clamps for some stuff.