[TheForge] h13 for chisels
John Newman
[email protected]
Mon Mar 25 18:15:01 2002
Anealling is its bad point. The only way I managed to aneal it at all was to
heat up in a pipe then put the hot pipe and chisel into vermiculite. It was
still hard but a NEW file would just cut it. Around here I can buy round stock
fairly inexpensivly but square stock has to be cut from plate so is very
expensive.
John Newman
Shannell wrote:
> Sounds like Im going to like this stuff, good for power hammer dies too Id
> guess, how hard is it to anneal, overnight in ashes enough?? What are the
> bad points?
>
> ----- Original Message -----
> From: "Dave Brown" <[email protected]>
> To: <[email protected]>
> Sent: Monday, March 25, 2002 10:42 PM
> Subject: Re: [TheForge] h13 for chisels
>
> > At 05:01 03/25/02 -0500, you wrote:
> >
> > >Any suggustions as to where to purchase H13, and what sizes and quanity
> is it
> > >available in. Thanks, Ralph
> > >
> > >Ralph Neumeister
> >
> > Ralph,
> >
> > Centaur Forge sells short pieces. They have H13 in 1/2" and 5/8" rounds
> in
> > 8", 10" & 12" pieces. Prices range from $5 to $7 ea. I'm told that it
> > comes in an annealed state and you can cut it through with a hack saw ...
> > you won't do this once you harden it.
> >
> > A good scrounge source (generally for 3/8" up to 1/2", maybe more) is
> > injection molding shops and factories. They use it for ejection
> > pins. They buy standard lengths with nice flat heads on them. When one
> in
> > use gets even the slightest bit worn they pull them and put new ones in
> > after cutting to length for the particular mold. They throw the cut off
> > ends and the old used pins in the dumpster. There's one member of UMBA
> > that lives near such a plant and they actually save all their reject pins
> > and cut offs for him. At our last informal gathering here in Green Bay he
> > brought a box full of H13 and we were free to take all we wanted. Great
> guy.
> >
> > Dave Brown
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________