I have used h13 for hot cuts etc. It is very good. I have not used s1 so I
cant compare to it ,but I think you will be pleased with h13.
Bob
----- Original Message -----
From: "Shannell" <[email protected]>
To: <[email protected]>
Sent: Sunday, March 24, 2002 5:11 PM
Subject: [TheForge] h13 for chisels


> Does anyone here use H13 for tooling, a local supplier reccomended it
above
> s1 as a good hot work tool steel, Ive heard of it being used before but
> wondered what its like for slitting chisels etc.
>