[TheForge] Canedy-Otto
northwoods
[email protected]
Sun Mar 24 09:12:01 2002
Dave, I use both a Cannedy-Otto forge and blower. I bought the forge
several years ago from a friend less the firepot, ducks nest, and all
associated parts. The forge was in like new shape, heavy cast construction,
about 3'by3', with the detachable arm on one side for the blower to bolt
on, also a water trough on the front. I happened to be looking at the
smithing stuff on e=bay one day and believe it or not, a guy out in MD had a
like new firepot and all the fixins, everything this forge needed, he was
also selling in another auction a like new CAnnedy-Otto "tiger" blower which
I also bought. Kinda worked out good for me, picked up everything I needed
to be able to use this forge in one feel swoop. I really like this setup and
have had no problems with it.
When I bought the blower it came with its own stand which I don't use. If
you have some use for it let me know.
T. Clark