S'OK, we all suffer from mind farts occasionally. My roomate fires up the
coffee pot at least once a week, and installs water, changes the filter, and
forgets to add the coffee. I've taken to loading it before I get to bed,
because I'll load it in the morning, and forget to turn it on. Pushing a
button, I can handle, as long as there are no other complications....
Phlip
Dave Brown wrote:
> It's lunch time and I've just come in from the shop. I relearned something
> just now... Sometimes we forget what we know and just plow on ahead
> without thinking first. I just did this. It wasn't a big deal, but it was
> certainly a reminder.
>
> I was making some shelf brackets for the shop and was making some right
> angle bends cold. No big deal, right? Right, except for one small
> detail. I had gotten some cold rolled 3/16"x3/4" from the "specials" bin
> at the steel yard. So, I cut some to the lengths I needed and proceeded to
> bend them in my HF Compact Bender. It was going smooth until just before I
> got to that 90 degree mark. Then .... #@*k, the bar broke. Did I remember
> what I should have remembered all along? Nope. I put another piece in the
> bender and ... #@*k it broke too. Then I remembered. "COLD ROLLED" It's
> been work hardened in the rolling process, that's why it was brittle and
> broke. So, into the propane forge for a while to anneal/normalize
> them. After they cooled they bent just fine.
>
> I should have known this would happen even before I tried bending the first
> piece. Well, actually I did know it would break, it just took to failed
> attempts to bend the cr stock to remind me of what I already knew.
>
> Dave Brown
> Heritage Smithing
> Green Bay, WI
> ABANA, UMBA, GoM, MODA, ARG
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________