> I may have a chance to get some steel  from a local rolling mill.I have
> gotten 1018 from them in the past.Would there be any advantage to getting
> 1010 or 1008.I use it for making mostly small decorative items.Would the
> lower carbon forge easier?Mark
> 
> 
> ---
> Mark & Sylvia Mondloch
> Silver Creek Pottery & Forge
> W6725 Hwy 144
> Random Lake ,Wi 53075
> [email protected]
> http://www.silvercreekpottery.com
> 
> 
> --- StripMime Report -- processed MIME parts ---
> multipart/mixed
>   text/plain (text body -- kept)
>   text/x-vcard
> ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
> 
>