[TheForge] argon vs argoshield for tig
Ray Miller
[email protected]
Fri Mar 15 10:00:08 2002
The sign of a true metal mangler!!!
;-)
Ray
Ralph Sproul wrote:
> Ray, Your always thinking.
>
>Ralph
>
>
>----- Original Message -----
>From: "Ray Miller" <[email protected]>
>To: <[email protected]>
>Sent: Friday, March 15, 2002 8:59 AM
>Subject: Re: [TheForge] argon vs argoshield for tig
>
>
>>What is argoshield? If that is 75/25 argon/CO2, then no, you don't want
>>to use it for TIG. You will get better results with
>>75/25 than straight argon on MIG. But 75/25 on TIG is not recommended.
>>An alternate for thin guage MIG is straight CO2, and then you could use
>>it for your beer tap as well........;-)
>>
>>Ray Miller
>>Cincinnati
>>Shannell wrote:
>>
>>>I Asked this q? a while back and thought I got an answer of yes, you can
>>>
>use
>
>>>argoshield with tig, I was just down at my welding supplyer and they were
>>>adamant that no you couldnt, I have mig and tig and wanted to save on an
>>>extra bottle as the tig is really not used a lot. Ive been using argon
>>>
>with
>
>>>my mig for about a year now but thought its time to go to argoshield.
>>>
>>>_______________________________________________
>>>http://mailman.qth.net/mailman/listinfo/theforge
>>>theforge mail list group photo site is
>>>http://www.photoaccess.com
>>>Login: [email protected]
>>>password: anvil
>>>___________
>>>
>>>
>>>
>>
>>
>>_______________________________________________
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login: [email protected]
>>password: anvil
>>___________
>>
>>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________
>
>
>