[TheForge] Re: Putting some blue color in iron
Mike Spencer
[email protected]
Thu Mar 14 20:43:59 2002
> What is the secret to getting a real nice blue that I have seen on
> some knives etc, should I be quenching in some magic brew or or or?
There's a method that involves immersing a cleaned and polished piece
in molton sodium and potassium nitrate. But that's all I know about
it. I'd like to hear more from anyone who's used this method myself.
- Mike
---
Michael Spencer Nova Scotia, Canada
[email protected]
http://home.tallships.ca/mspencer/