[TheForge] non-ferrous metals
Woolley
[email protected]
Sun Mar 10 17:28:02 2002
Woolley wrote:
>
> Bob Bergman wrote:
> >
> > It is a 81 page book, short and to the point. It has metallurgical
> > information but not text book type.Materials are described by use,
> > composition,properties and welding procedures. It has a spark test
> > diagram. It covers ferrous,non-ferrous,tempering and hardening.A good
> > quick reference book. Bob
>
> Bob,
>
> Thanks alot, that was a help help.
>
> Cheers,
> Bill Woolley
Bob
That was not only a help help it was a great help.