[TheForge] unique anvil
evelyn hart
[email protected]
Sat Jun 29 13:50:01 2002
The hole in an anvil has been discussed on theforge several times. The hole
was used to handle the anvil when the anvil was being forged/made.
Bobby Hart
Hush Puppy Forge
Griffin, GA
OBG, AFC
----- Original Message -----
From: "Phlip" <[email protected]>
To: <[email protected]>
Sent: Saturday, June 29, 2002 1:01 AM
Subject: Re: [TheForge] unique anvil
>
>
>
> > I am considering buying a 250 lb. anvil. I did not see any markings
other
> > than what apears to be a "P'' below the horn on the bottom of the base
on
> > the left and an "R" on the base on the right. It is a London Pattern
with
> > decent edge and face(one significant ding on edge).The unique thing is
> that
> > there is a hole going crosswise thru the anvil at the mid point . The
hole
> > is about 1 to 1.5 inch in diameter.
> > It appears to have been made this way. Can someone tell me more about
this
> > thing.It is far enough below the face to not weaken it. The price is
> $1.50
> > lb.
>
> Sounds like it might be a tie-down. I've seen a couple anvils with holes
> like that, and that's all I could figure.
>
> Phlip
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>