isnt the atmosphere mostly nitrogen?
----- Original Message -----
From: "Jeff Harding" <[email protected]>
To: <[email protected]>
Sent: 23 June, 2002 11:00 PM
Subject: Re: [TheForge] enameling
> Or a kiln in a nitrogen atmosphere? Though I'm not certain what the
> nitrogen would do at high temps, may be a problem there too...
>
>
> ----- Original Message -----
> From: "Demon Buddha" <[email protected]>
> To: <[email protected]>
> Sent: Sunday, June 23, 2002 10:33 AM
> Subject: Re: [TheForge] enameling
>
>
> >
> >
> > Bob Smolen wrote:
> > >
> > > I heard one of the demonstrators at the ABANA conference enameled
> a piece of
> > > hot iron by applying granulated glass(?) I think. It was easy and
> very nice
> > > looking. Can someone describe the process and result of enameling
> in the
> > > context of forged work.
> >
> > I've never done enameling on iron, but have on brass, copper,
> > and precious metals. For these, the process is as follows:
> >
> > The surfaces to be enameled should be clean and free of oxides
> > (is this so for iron?). All areas where enamel is not wanted
> > should be masked off with a material whose name I have forgotten,
> > though it is maddeningly on the tip of my tounge but won't come.
> > It is a bluish paint that dries in the air (sorry for the poor
> > memory). I'm wondering if one could substitute china white oy
> > yellow ochre. Anyone?
> >
> > Sprinkle the frit (pulverised glass) onto the area to receive
> > enamel and place into the heat source. If you are enameling a
> > curved piece, use gum arabic on the surface. It will act as a
> > glue for the frit. If you are enameling a curved surface, you
> > paint a thin coat of gum arabic onto it and then sprinkle the
> > frit on the tacky gum. Fire as usual.
> >
> > As the temperature comes up, the frit will melt. As I recall
> > the enameling frits melt at about 1200 F. I've done mine on a
> > temperature controlled enameling kiln, so I did not have to be
> > vigilant for over heat. The frit will melt and the surface
> > appearance will take on that "wet" look. At that time the work
> > should be removed and allowed to cool SLOWLY, preferably in a
> > still air box so that the new enamel doesn't spall due to
> > too-violent contraction. You can further reduce the rate of
> > cooling by setting the hot work on kiln furniture. Preheating
> > the furniture to, say, 500 degrees will further decrease the
> > thermal shock to the work. All this extra care should be
> > predicated on the desired outcome. If you don't mind cracked
> > or spalled enamel, then don't worry about it. Some may even
> > want this effect as it has its own appeal.
> >
> > What you can do then, if you are doing cloisonn�, is grind the
> > surface of the glass until the wires show through. Refire as
> > per above and you will have a nicely defined set of borders
> > between regions of differing color.
> >
> > Cloisson�. in cross section for those not familiar with it:
> >
> > Wire--------| |------Frit
> > | |
> > _____________|_________ ___|______
> > | |___________O_________O________| | <--- metal bezel
> > |__________________________________| <--- metal
> >
> > First firing
> >
> >
> > Wire--------| |------Frit
> > | |
> > _____________|_________ ___|______
> > | |___________U_________U________| | <--- metal bezel
> > |__________________________________| <--- metal
> >
> > Ground and refired
> >
> > Please forgive horrible ASCII artwork.
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>