I probably round out my slitting and drifting tooling for starters, maybe
make some round and square punches.  I purchased one each 1/4" x 3', 3/8" x
3' and 1/2" x 3' and it was 44.00 plus shipping!  PLEASE give me the address
of Burgon Tool Steel!!!!!!!!!!!!!!!!!!!!!!!
Yes, I am going to Ian's......see you there.  I"ll have to bring several
handkerchiefs to ward off the drool when I ask you about your recent
acquisitions!
Chris

----- Original Message -----
From: Ralph Sproul <[email protected]>
To: <[email protected]>
Sent: Thursday, June 20, 2002 10:39 PM
Subject: Re: BLACKSMITHING was [TheForge] Patriotic rant....


>         Chris, what are you going to make??  decorative chisels? or
magician
> tooling? or something else?
>         Are you going to Ian's workshop in Saxton's River on Sat?   Ian is
> going to show how he's been making thumb latches all by power hammer for
> starters.......nice latches, you'd swear they were done by
> hand..........maybe the 24 years of practice has something to do with it.
> :-)
>         By the way, did I give you the address of Burgon Tool Steel? they
> sell S7 for much less than what MSC does.
>
> Ralph Sproul - Bear Hill Blacksmith
> Webster, NH
>
>

>