[TheForge] Mastermyr - Fire Grid
Rob Fertner
[email protected]
Tue Jun 4 17:12:00 2002
YOU DA MAN!!
Well done and Thanks again.
Bless you,
Rob
----- Original Message -----
From: "April & Bill Clemens" <[email protected]>
To: <[email protected]>
Sent: Tuesday, June 04, 2002 12:22 PM
Subject: Re: [TheForge] Mastermyr - Fire Grid
> Rob, et al,
>
> It's Done!!!! Even a quick and dirty stand.
>
> I'm leaving in a few minutes to meet Roger in Harrisburg. I'll post
> pictures this evening when I return for those not going to the
> Conference, like me.
>
> Bill
>
> April & Bill Clemens wrote:
>
> > Rob, et al,
> >
> > Only 8 more rivets to go! Might even have time to make that stand
> > tomorrow, after the rivets finishing. Have to leave here by 1 pm to
> > meet Roger at 3 pm. No pictures tonight, I'll post some tomorrow.
> >
> > Bill
> >
> >
> > Rob Fertner wrote:
> >
> >> Bill,
> >> No, I haven't thought of a way to display it. :-(
> >> I'm glad you did. :-)
> >>
> >> To All:
> >> I have 37 items in my possession (including the chest) at this time.
> >> I plan on leaving Wichita on the 4th. So if any items are in transit
> >> I hope they get here soon.
> >>
> >> Once again thanks to everyone involved.
> >> Rob
> >>
> >> ----- Original Message -----
> >> From: "April & Bill Clemens" <[email protected]>
> >> To: <[email protected]>
> >> Sent: Sunday, June 02, 2002 9:02 PM
> >> Subject: Re: [TheForge] Mastermyr - Fire Grid
> >>
> >>
> >>> Rob, Phlip, et al
> >>>
> >>> Just posted a new picture of my progress. The eye swivel was lots of
> >>> fun. Tried your way Phlip and then my idea, neither worked. Finally
I
> >>> formed the head and then prebent the hook into a U shape with the wrap
> >>> sticking out at 90 degree. I then slid it through the plate, heated
> >>> it,
> >>> closed the eye and did the wrap. Only 5 more grid rods to forge and
33
> >>> rivets to go. I'm planning to meet Roger at 3pm Tuesday, so I have
a
> >>> day and 1/2 to complete it.
> >>>
> >>> Rob do you know how you're planning to display it? Do you have
> >>> something to hang it from? If I have time I'll make a simple stand
> >>> that
> >>> will support the top plate and chains with the Fire Grid setting on
> >>> the
> >>> ground.
> >>>
> >>> Bill
> >>>
> >>> Phlip wrote:
> >>>
> >>>> Not really, other than decide which way you're going to do it
> >>>> before you
> >>>> start. I suspect wrapping the knot first would be easiest, then
> >>>> peen over
> >>>> the rivet head afterwards, with the 4 cornered plate.
> >>>>
> >>>> But, it's up to you.
> >>>>
> >>>> Phlip
> >>>>
> >>>>
> >>>>
> >>>> ----- Original Message -----
> >>>> From: "April & Bill Clemens" <[email protected]>
> >>>> To: <[email protected]>
> >>>> Sent: Saturday, June 01, 2002 1:37 PM
> >>>> Subject: Re: [TheForge] Mastermyr - Fire Grid
> >>>>
> >>>>
> >>>>> Phlip,
> >>>>>
> >>>>> Any comments on my swivel drawing before I go out to forge it?
> >>>>>
> >>>>> A swivel, 2 forge welds, 10 grid pieces, 2 thin strips and 37
> >>>>> rivets to
> >>>>> go. Gonna be a busy weekend.
> >>>>>
> >>>>> Bill
> >>>>>
> >>>>> April & Bill Clemens wrote:
> >>>>>
> >>>>>> Phlip, rob, et al
> >>>>>>
> >>>>>> No smithing today...yet! Had to get ready for a back hoe coming
> >>>>>> tomorrow instead of next week to dig a footer at the back of my
> >>>>>> house. Planning to go out now for a few hours work. Once he gets
> >>>>>> started tomorrow I hope to forge while he digs.
> >>>>>>
> >>>>>> Posted the three pics of Steve's Chest in a folder labeled
Mastermyr
> >>>>>> Photos along with my Fire Grid Pics. Also posting a drawing
> >>>>>> there of
> >>>>>> the top swivel. Looks like it has a rivet like head with the eye
> >>>>>> formed and the end tapered and wrapped around. Your thoughts.
> >>>>>> (And I
> >>>>>> promise to read your thoughts Phlip BEFORE I FORGE AHEAD).
> >>>>>>
> >>>>>> Bill
> >>>>>>
> >>>>>>
> >>>>>> Larry and Pat Brown wrote:
> >>>>>>
> >>>>>>> Pictures look good!!
> >>>>>>> Larry Brown
> >>>>>>>
> >>>>>>> At 09:56 PM 5/30/2002 -0600, you wrote:
> >>>>>>>
> >>>>>>>> That's fine with me, but I find that site slow. Slightly lower
> >>>>>>>> resolution pics
> >>>>>>>> are up on my web page:
> >>>>>>>> http://www.frii.com/~sos
> >>>>>>>>
> >>>>>>>> Steve
> >>>>>>>>
> >>>>>>>
> >>>>>>>
> >>>>>>> _______________________________________________
> >>>>>>> http://mailman.qth.net/mailman/listinfo/theforge
> >>>>>>> theforge mail list group photo site is
> >>>>>>> http://www.photoaccess.com
> >>>>>>> Login: [email protected]
> >>>>>>> password: anvil
> >>>>>>> ___________
> >>>>>>>
> >>>>>>>
> >>>>>>>
> >>>>>>>
> >>>>>> _______________________________________________
> >>>>>> http://mailman.qth.net/mailman/listinfo/theforge
> >>>>>> theforge mail list group photo site is
> >>>>>> http://www.photoaccess.com
> >>>>>> Login: [email protected]
> >>>>>> password: anvil
> >>>>>> ___________
> >>>>>>
> >>>>>>
> >>>>>>
> >>>>>>
> >>>>> _______________________________________________
> >>>>> http://mailman.qth.net/mailman/listinfo/theforge
> >>>>> theforge mail list group photo site is
> >>>>> http://www.photoaccess.com
> >>>>> Login: [email protected]
> >>>>> password: anvil
> >>>>> ___________
> >>>>>
> >>>>>
> >>>>>
> >>>> _______________________________________________
> >>>> http://mailman.qth.net/mailman/listinfo/theforge
> >>>> theforge mail list group photo site is
> >>>> http://www.photoaccess.com
> >>>> Login: [email protected]
> >>>> password: anvil
> >>>> ___________
> >>>>
> >>>>
> >>>>
> >>>>
> >>>
> >>> _______________________________________________
> >>> http://mailman.qth.net/mailman/listinfo/theforge
> >>> theforge mail list group photo site is
> >>> http://www.photoaccess.com
> >>> Login: [email protected]
> >>> password: anvil
> >>> ___________
> >>>
> >>>
> >>
> >>
> >> _______________________________________________
> >> http://mailman.qth.net/mailman/listinfo/theforge
> >> theforge mail list group photo site is
> >> http://www.photoaccess.com
> >> Login: [email protected]
> >> password: anvil
> >> ___________
> >>
> >>
> >>
> >>
> >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
> >
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>