[TheForge] Pure Iron

Andrew Vida [email protected]
Tue Jul 30 21:59:00 2002


I've heard they were giving up on it, but I have not confirmed this with =
Mike Schermerhorn.

Shame.  It's very nice for many things, especially anything =
non-structural.

-----Original Message-----
From: John Chobrda [mailto:[email protected]]
Sent: Tuesday, July 30, 2002 4:55 AM
To: The forge
Subject: [TheForge] Pure Iron


    I hope it's not true but I heard a rumor that the outfit that
imports pure iron might be having some problems, and calling it quits.
Does anyone know whats really going on.
Thanks
John C.