[TheForge] Decorative heads

Ray Miller [email protected]
Tue Jul 23 09:15:00 2002


I have welded them and they were fine. I have not forged them. If you 
keep them on a stud that should hold the thread shape, or you might have 
to run a tap through it just to clean the threads up.

Ray Miller
Cincinnati

Shannell Sugrue wrote:

>I like that idea, but if I forge them out a bit the thread would probably
>get distorted, even if I had it on a stud when I forged it, or mabey not,
>have you tried forging these?
>
>----- Original Message -----
>From: "Ray Miller" <[email protected]>
>To: <[email protected]>
>Sent: 23 July, 2002 11:01 AM
>Subject: Re: [TheForge] Decorative heads
>
>
>>Why not start with a covered nut or acorn nut? I have gotten them from
>>my fastener supplier.
>>The brass ones are very attractive.
>>Ray Miller
>>Cincinnati
>>
>>Shannell Sugrue wrote:
>>
>>>Does anyone have a method for making decorative heads to fit over the top
>>>
>of
>
>>>a nut on a stud? I was thinking of just making a die from the nut shape
>>>
>and
>
>>>pounding it into a blank and rounding off the top, but then how to attach
>>>it? epoxy mabey. Anyone ever use the epoxy "knead it" (the 2 pak clay
>>>
>like
>
>>>stuff) and mold some of that over the head and paint it? Seems too much
>>>
>like
>
>>>cheating :)
>>>
>>>_______________________________________________
>>>http://mailman.qth.net/mailman/listinfo/theforge
>>>theforge mail list group photo site is
>>>http://www.photoaccess.com
>>>Login:  [email protected]
>>>password:  anvil
>>>___________
>>>
>>>
>>>
>>
>>
>>_______________________________________________
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login:  [email protected]
>>password:  anvil
>>___________
>>
>>
>>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  [email protected]
>password:  anvil
>___________
>
>
>



--- StripMime Report -- processed MIME parts ---
multipart/alternative
  text/plain (text body -- kept)
  text/html
The reason this message is shown is because the post was in HTML
or had an attachment. Attachments are not allowed.
Please post in Plain-Text only.---