Thu Jul 11 10:08:00 2002
I have a bundle of 1/2" round S-7 for cheap (5 bucks for a ~2ft stick)
Don't know of many h20 hardening hot-work steels.
Steve
-----Original Message-----
From: Bob Rackers [mailto:[email protected]]
Sent: Wednesday, July 10, 2002 7:43 PM
To: TheForge
Subject: [TheForge] Looking for round S-1
Anyone know where to find 1/2" diameter S-1?
Looking for a water hardening hot work steel if S-1 isn't available.
Bob