1/2" round is approximately 0.668 pounds per foot * 3 feet = 2.004 pounds *
$3.45 = $6.92 + shipping
Is that math correct? (That seems reasonable, depending on the shipping, of
course.)

If this isn't 1/2" drill rod (I'm assuming it's not), any idea of the allowable
tolerance on 1/2" round?

Bob

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Dick Nietfeld
Sent: Wednesday, July 10, 2002 10:48 PM
To: [email protected]
Subject: Re: [TheForge] Looking for round S-1


Bob, the following is an e-mail from Pete Stanaitis:

Cincinnati Tool Steel Company
5162 28th Ave
Rockford, Il, 61125

1-815-226-8800

They have a national Wats #: 1-800-435-0717, so they must have offices
in other places, too.  The last time I bought some 1/2" round, it was
$3.45 per pound plus UPS COD shipping costs.

Dick Nietfeld
Shady Grove Blacksmith Shop
Grand Island, NE