[TheForge] pyrometer question
Fiorini & Skiles
[email protected]
Thu Jul 4 22:01:03 2002
You can buy a pyrometer to measure mokume-gane from most ceramic suppliers.
Mn Clay is one. I used a pyrometer for awhile, but decided to trust my eyes
instead. When you use a cheaper pyrometer in a gas forge I would suggest
using a ceramic tube to help keep the probe from melting. For Damascus, get
a good reduced atmosphere going and use a 1/4" mild steel touch rod for
measuring the welding temperature. When the rod sticks to your billet, it
is ready to weld. I have found that in order to have complete success with
mokume you should go to a heat treat furnace for the diffusion.
Bill
----- Original Message -----
From: <[email protected]>
To: <[email protected]>
Sent: Thursday, July 04, 2002 1:03 PM
Subject: [TheForge] pyrometer question
> i am considering purchaseing a pyrometer to measure the temp in my gas
> forge.i would like to use it to make mokume and demascus.does anyone out
> there use or have any info or webs site.thanks
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>