The link didn't come up, but bronze is amenable to oxy-acet, MIG and TIG
welding. You can either forge out some of the original material to use as
filler rod or search out a matching alloy for color matching. It is not
much of a problem except that you may have to grind through the "rind" that
surrounds some castings ( especially sand castings). Pete F
> >
> >Hello Chuck.
> >
> > I found you on the web and see you do metalwork among other things. I
> >desperatly need to learn how to weld small pieces of cast bronze. We have
> >no problem getting them cast here, but no one wants to put em together. I
> >offer in trade the key to making the old Italian violin varnish. Its
> >contained in a book called Michalmans Violin varnish. Im not sure about the
> >spelling, my copy is at the house. I found it via inter-library loan when I
> >was in the states. I couldnt find the materials when I lived in New
> >Orleans, but in the eastern Mediterranean all the old style market places
> >have the materials in gunny sacks.
> > If you can help me it would be greatly appreciated. Though lessons are
> >best, I have the ability to lean from books. The pieces in question can be
> >viewed at http://www.enyoart.biz. Most of the bronze seen there is cast
> >from three to six molds and then joined to fit the glass piece. Its old
> >style bronze, 95% copper 5% tin, if I remember correctly. The artist has
> >some experience with gold jewelry, and I feel we can do the job with the
> >right tools and chemistry,
> >
> >Thanks
> >Chuck
>
>
>
>Dave Mudge [email protected]
>don't reply to me, reply to [email protected]
>
>
>
>--- StripMime Report -- processed MIME parts ---
>multipart/alternative
> text/plain (text body -- kept)
> text/html
>The reason this message is shown is because the post was in HTML
>or had an attachment. Attachments are not allowed.
>Please post in Plain-Text only.---
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________