[TheForge] Pure Iron

RW [email protected]
Tue Jan 29 20:35:01 2002


I have noticed PI has "clay-like qualities" that I like in some applications
and not in others.
RW
----- Original Message -----
From: John Chobrda <[email protected]>
To: The forge <[email protected]>
Sent: Tuesday, January 29, 2002 2:01 PM
Subject: [TheForge] Pure Iron


> Today I forged a fireplace poker out of a piece of 1/2 in. sq. pure iron
> I picked up a while ago. I have mixed feelings about this material,
> forging was no problem except for the fact that the stock bent where hot
> roll wouldn't (away from the color zone) also I wanted to put a twist in
> the center of the poker, and that was a learning experiance. I put a
> piece in the vice and tried to twist it cold, it does not behave like
> hot roll. Has anyone else experianced this? At 5 to 6 times the cost of
> HR I don't think I'll use this for any large projects (gates, Fences,
> etc.).
>
> John C.
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>