[TheForge] welding 1 1/2" square
RW
[email protected]
Thu Jan 24 12:43:24 2002
That's a keeper Darrell. :]
----- Original Message -----
From: Darrell <[email protected]>
To: <[email protected]>
Sent: Thursday, January 24, 2002 12:36 PM
Subject: Re: [TheForge] welding 1 1/2" square
> How about forge welding?
> Darrell
>
> http://www.machinemaster.com
>
>
> ----- Original Message -----
> From: "RW" <[email protected]>
> To: <[email protected]>
> Sent: Thursday, January 24, 2002 5:31 AM
> Subject: [TheForge] welding 1 1/2" square
>
>
> > Is it possible to butt weld 1 1/2" solid mild steel with a 230 amp max.,
AC
> > 220v welder?
> > It does not need to be a "structural weld", just to hold a fireplace
grate
> > frame together.
> > I tried it with a #7 oxy/acet tip which is for 1 1/4" max and it is not
much
> > better than if I had used chewing gum.
> > RW
> >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>