[TheForge] Welding copper (was:fountains)

Peter Fels and Phoebe Palmer [email protected]
Wed Jan 23 22:58:00 2002


At 12:03 PM 1/23/02, you wrote:

Yup, the TIG will make really nice welds in almost any metal...the cost 
disappears when you consider the finishing time you save.
In reality, you can do it with an acet/oxy torch too, but the learning 
curve is steeper.
Maybe you could  trade the pills for a Henrob......Pete




>Ok Pete, you are right.  The pills didn't work.   Will a TIG do the job?
>
>
>  :)
>
>Adam
>
>
>At 10:22 PM 1/22/2002 -0800, you wrote:
>>At 09:43 PM 1/22/02, you wrote:
>>
>>
>>The Henrob is an odd little  low pressure oxy-acet torch  with a clunky 
>>cast aluminum pistol grip handle that looks like something made by some 
>>guys in their garage after WW2.  It is kind of a throwback to early 
>>oxy/acet. They used to be sold under the name Dillon Mark 3.
>>They are promoted with the  level of hyperbole generally reserved for 
>>guaranteed diet pills that enlarge your member.  A fair part of the promo 
>>material is sheer BS.  For example, they are a lousy cutting torch and 
>>the flame isn't any hotter than other torches.
>>On the other hand, they do have a very nice soft, low velocity  flame 
>>that is good for small welding...IF you are already a good welder.
>>I think you can do almost all of what a henrob does with a good small 
>>torch run at low pressures, perhaps with properly modified tips.
>>Yes , I own one. You can often pick them up cheap from guys who see them 
>>demoed at the fair or the small aircraft shows, bring them home, and find 
>>they are short a few months of practice....so they put them on the shelf 
>>in the garage...and there they sit.
>>Save your money for a TIG, is my advice.........Pete F
>>
>>
>>
>>>I think the best answer to that question is, "yes!"
>>>The Henrob is a brand of torch, but it is designed differently from most
>>>torches... I sure wish I had one!
>>>I did a search for Henrob Torch and came up with quite a few sites that
>>>would love to sell you one... one of which is
>>>http://www.interking.com/m/o/henrob_torch.html  I know nothing of this
>>>company, it was just an easy link.
>>>
>>>
>>>At 11:28 PM 1/22/02 -0600, you wrote:
>>> >Is a "henrob" a special torch, or the brand name?
>>> >
>>> >Larry
>>> >
>>> >Roger R Degner wrote:
>>> >
>>> >> I have welded using a henrob oxy/acet torch using a piece of the parent
>>> >> material or copper electric wire as the filler
>>> >> Roger R Degner
>>> >> Franklin,Minn,USA
>>> >
>>> >_______________________________________________
>>> >http://mailman.qth.net/mailman/listinfo/theforge
>>> >theforge mail list group photo site is
>>> >http://www.photoaccess.com
>>> >Login:  [email protected]
>>> >password:  anvil
>>> >___________
>>> >
>>> >
>>> >
>>>-----------------------------------------------------
>>>Click here for Free Video!!
>>>http://www.gohip.com/freevideo/
>>>
>>>_______________________________________________
>>>http://mailman.qth.net/mailman/listinfo/theforge
>>>theforge mail list group photo site is
>>>http://www.photoaccess.com
>>>Login:  [email protected]
>>>password:  anvil
>>>___________
>>
>>
>>_______________________________________________
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login:  [email protected]
>>password:  anvil
>>___________
>>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  [email protected]
>password:  anvil
>___________
>