[TheForge] Welding copper (was:fountains)
Larry
[email protected]
Wed Jan 23 00:31:12 2002
This is what I had hoped for. Have to try it and see how it works for me.
Larry
H and P Foster wrote:
> I'm not very high tech when it comes to this kind of thing so I
> experimented, and found that plumbers flux works . You have to be careful
> with the torch and using a small tip size, bring the two parts up to temp
> and presto, they go together very nicely, leaving you with a bond where you
> can't tell one part from the other.
>
> Harry Foster
> Rusty Dog Forge